The heated ceramic shell is placed into a steel container and held in place with sand. |
| Molten bronze of approximately 2,200 F is prepared for the pour. |
|
| |
Pouring molten bronze is a team effort. |
| The cast piece remains in sand allowing the bronze to solidify and the molecules to align in a certain matrix. |
|